規(guī)格級別: | --- | 外觀顏色: | --- |
用途概述: | 廣泛使用在汽車內(nèi)部零件、事務機器、通信器材、家電用品及照明設備上。典型應用范圍:手機外殼、計算機和商業(yè)機器殼體、電器設備、草坪園藝機器、汽車零件儀表板、內(nèi)部裝修以及車輪蓋 | ||
備注說明: | 特性:阻燃V0,耐高溫 |
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
物理性能 | 比重 | --- | ASTM D-792 | 1.18 | --- |
吸水率 | --- | ASTM D-570 | 0.1 | % | |
模具收縮率 | 3.2mm | ASTM D-955 | 4-6 | E-3 | |
機械性能 | 拉伸強度(屈伏點) | --- | ASTM D-638 | 63 | Mpa |
拉伸率(斷裂點) | --- | ASTM D-638 | 40 | % | |
拉伸模量 | --- | ASTM D-638 | - | Mpa | |
彎曲強度 | --- | ASTM D-790 | 102 | Mpa | |
彎曲模量 | --- | ASTM D-790 | 2653 | Mpa | |
沖擊強度缺口 | 23℃ | ASTM D-256 | 533 | J/m | |
洛氏硬度 | --- | D785 | 123 | R | |
電氣性能 | 損耗因數(shù) | 1MHz | ASTM D-150 | - | --- |
介電常數(shù) | 1MHz | ASTM D-150 | - | --- | |
體積電阻 | --- | ASTM D-150 | 1.0E+17 | Ohm-cm | |
表面電阻 | --- | ASTM D-257 | 1.0E+16 | Ohm-cm | |
熱 性 能 | 阻燃性 | --- | UL-94 | V-0 | --- |
阻燃性 | --- | UL-94 | 1.6 | mm | |
熱變形溫度 | 0.45Mpa | ASTM D-648 | 104 | ℃ | |
熱變形溫度 | 1.8Mpa | ASTM D-648 | 95 | ℃ | |
維卡軟化點 | --- | ASTM D-1525 | 112 | ℃ | |
線膨脹系數(shù) | --- | E-831 | - | 1/℃ | |
UL長期使用溫度 | 含沖擊 | UL-746B | 75 | ℃ | |
UL長期使用溫度 | 無沖擊 | UL-746B | 85 | ℃ |
PC/ABS在PCT(Pressure Cooker Test)測試中,在95%RH,100℃高溫高濕環(huán)境1000h后,該PC/ABS中的PC相仍然保持90%以上的分子量,未發(fā)生嚴重的水解;而合金的沖擊性能僅下降15%,相比一般PC/ABS提高30%以上的性能。此外,該系列材料為了適應儀表板薄壁化的要求,降低了材料在高剪切下的粘度,克服了過去片面提高溫度來提高材料流動性所帶來的材料熱分解的弊端。
新一代耐水解穩(wěn)定性PC/ABS材料,由于具有良好的耐水解性和熱穩(wěn)定性,甚至可以進行回收利用。當添加25%以下的回收料以后,材料的多軸沖擊性能僅下降11%,并且為韌性斷裂,充分顯示了新一代PC/ABS的優(yōu)越性能。同時該系列材料也經(jīng)過了大眾實驗室的評測,在80%RH,90℃高溫高濕水解600h后,缺口沖擊強度僅下降8.5%。
規(guī)格級別: | --- | 外觀顏色: | --- |
用途概述: | 廣泛使用在汽車內(nèi)部零件、事務機器、通信器材、家電用品及照明設備上。典型應用范圍:手機外殼、計算機和商業(yè)機器殼體、電器設備、草坪園藝機器、汽車零件儀表板、內(nèi)部裝修以及車輪蓋 | ||
備注說明: | 特性:阻燃V0,耐高溫 |
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
物理性能 | 比重 | --- | ASTM D-792 | 1.18 | --- |
吸水率 | --- | ASTM D-570 | 0.1 | % | |
模具收縮率 | 3.2mm | ASTM D-955 | 4-6 | E-3 | |
機械性能 | 拉伸強度(屈伏點) | --- | ASTM D-638 | 63 | Mpa |
拉伸率(斷裂點) | --- | ASTM D-638 | 40 | % | |
拉伸模量 | --- | ASTM D-638 | - | Mpa | |
彎曲強度 | --- | ASTM D-790 | 102 | Mpa | |
彎曲模量 | --- | ASTM D-790 | 2653 | Mpa | |
沖擊強度缺口 | 23℃ | ASTM D-256 | 533 | J/m | |
洛氏硬度 | --- | D785 | 123 | R | |
電氣性能 | 損耗因數(shù) | 1MHz | ASTM D-150 | - | --- |
介電常數(shù) | 1MHz | ASTM D-150 | - | --- | |
體積電阻 | --- | ASTM D-150 | 1.0E+17 | Ohm-cm | |
表面電阻 | --- | ASTM D-257 | 1.0E+16 | Ohm-cm | |
熱 性 能 | 阻燃性 | --- | UL-94 | V-0 | --- |
阻燃性 | --- | UL-94 | 1.6 | mm | |
熱變形溫度 | 0.45Mpa | ASTM D-648 | 104 | ℃ | |
熱變形溫度 | 1.8Mpa | ASTM D-648 | 95 | ℃ | |
維卡軟化點 | --- | ASTM D-1525 | 112 | ℃ | |
線膨脹系數(shù) | --- | E-831 | - | 1/℃ | |
UL長期使用溫度 | 含沖擊 | UL-746B | 75 | ℃ | |
UL長期使用溫度 | 無沖擊 | UL-746B | 85 | ℃ |
規(guī)格級別: | --- | 外觀顏色: | --- |
用途概述: | 廣泛使用在汽車內(nèi)部零件、事務機器、通信器材、家電用品及照明設備上。典型應用范圍:手機外殼、計算機和商業(yè)機器殼體、電器設備、草坪園藝機器、汽車零件儀表板、內(nèi)部裝修以及車輪蓋 | ||
備注說明: | 特性:阻燃V0,耐高溫 |
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
物理性能 | 比重 | --- | ASTM D-792 | 1.18 | --- |
吸水率 | --- | ASTM D-570 | 0.1 | % | |
模具收縮率 | 3.2mm | ASTM D-955 | 4-6 | E-3 | |
機械性能 | 拉伸強度(屈伏點) | --- | ASTM D-638 | 63 | Mpa |
拉伸率(斷裂點) | --- | ASTM D-638 | 40 | % | |
拉伸模量 | --- | ASTM D-638 | - | Mpa | |
彎曲強度 | --- | ASTM D-790 | 102 | Mpa | |
彎曲模量 | --- | ASTM D-790 | 2653 | Mpa | |
沖擊強度缺口 | 23℃ | ASTM D-256 | 533 | J/m | |
洛氏硬度 | --- | D785 | 123 | R | |
電氣性能 | 損耗因數(shù) | 1MHz | ASTM D-150 | - | --- |
介電常數(shù) | 1MHz | ASTM D-150 | - | --- | |
體積電阻 | --- | ASTM D-150 | 1.0E+17 | Ohm-cm | |
表面電阻 | --- | ASTM D-257 | 1.0E+16 | Ohm-cm | |
熱 性 能 | 阻燃性 | --- | UL-94 | V-0 | --- |
阻燃性 | --- | UL-94 | 1.6 | mm | |
熱變形溫度 | 0.45Mpa | ASTM D-648 | 104 | ℃ | |
熱變形溫度 | 1.8Mpa | ASTM D-648 | 95 | ℃ | |
維卡軟化點 | --- | ASTM D-1525 | 112 | ℃ | |
線膨脹系數(shù) | --- | E-831 | - | 1/℃ | |
UL長期使用溫度 | 含沖擊 | UL-746B | 75 | ℃ | |
UL長期使用溫度 | 無沖擊 | UL-746B | 85 | ℃ |